Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | >= 2.71 J | >= 2.00 ft-lb | ASTM D5420 |
S&E Specialty Polymers GPP1005HF Series PP Application: UL94 V-2, Flame-retardant polypropylene compounds for injection molding applications.Information provided by S&E Specialty Polymers |
|||
Dart Drop, Total Energy | 2.71 J | 2.00 ft-lb | ASTM D3420 |
LyondellBasell Alathon® L4907 High Density Polyethylene ApplicationsALATHON L 4907 is a high molecular weight high density copolymer with broad dimodal molecular weight distribution. This resin exhibits high density and stiffness and is designed for gro.. |
|||
Dart Drop, Total Energy | 2.71 - 14.9 J | 2.00 - 11.0 ft-lb | Average value: 8.59 J Grade Count:3 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |