Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 47.5 J | 35.0 ft-lb | Conditioned; ASTM D3763 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
Dart Drop, Total Energy | 47.5 J | 35.0 ft-lb | Instrumented; ASTM D3763 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |