Dart Drop, Total Energy 56.5 - 62.1 J

@Temperature -29.0 - -29.0 °C
41.7 - 45.8 ft-lb

@Temperature -20.2 - -20.2 °F
Average value: 52.3 J Grade Count:3
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Dart Drop, Total Energy 56.5 - 62.1 J

@Thickness 3.20 - 3.20 mm
41.7 - 45.8 ft-lb

@Thickness 0.126 - 0.126 in
Average value: 52.3 J Grade Count:3
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Dart Drop, Total Energy 56.5 J
41.7 ft-lb
3.39 m/sec; ASTM D3763
Styron CALIBREâ„¢ IM 401-11 Polycarbonate Resin
Overview: CALIBREâ„¢ IM 401-11 Impact Modified Polycarbonate resin is available in opaque formulations that offer benefits ranging from superior low temperature impact strength to easy process wi..