Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dart Drop, Total Energy = 59.2 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 49.0 - 80.2 J

@Temperature -40.0 - 0.000 °C
36.1 - 59.2 ft-lb

@Temperature -40.0 - 32.0 °F
Average value: 55.4 J Grade Count:2
Overview of materials for Polycarbonate/PET Polyester Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values..
Dart Drop, Total Energy 49.0 - 80.2 J

@Thickness 3.20 - 3.20 mm
36.1 - 59.2 ft-lb

@Thickness 0.126 - 0.126 in
Average value: 55.4 J Grade Count:2
Overview of materials for Polycarbonate/PET Polyester Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values..