Mechanical Properties Metric English Comments
Dart Drop, Total Energy >= 8.13 J
>= 6.00 ft-lb
ASTM D5420
S&E Specialty Polymers GPP6025 PP
Application: Specially engineered, low bloom, low specific gravity, flame retardant polypropylene compound designed with halogen based technology. Exhibits a unique balance of high flexural modulus ..