Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers GPP6025 PP

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer S&E Specialty Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers GPP6025 PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Specially engineered, low bloom, low specific gravity, flame retardant polypropylene compound designed with halogen based technology. Exhibits a unique balance of high flexural modulus and high impact.  It is designed for use in injection molded industrial power supply systems and to meet their stringent criterion. The superior balance of flow, allows the material to maintain excellent aesthetics over long flow lengths.  Available in a wide spectrum of colors.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.27 - 1.31 g/cc
1.27 - 1.31 g/cc
ASTM D792
Melt Flow 16 - 20 g/10 min
16 - 20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 17.2 MPa
>= 2500 psi
ASTM D638
Elongation at Break >= 50 %
>= 50 %
ASTM D638
Flexural Modulus >= 1.65 GPa
>= 240 ksi
ASTM D790
Dart Drop, Total Energy >= 8.13 J
>= 6.00 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Flammability Test 5.0

@Thickness 1.59 mm
5.0

@Thickness 0.0625 in
Users viewing this material also viewed the following: