Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 0.678 J | 0.500 ft-lb | ASTM D3029 |
Total 680 Polystyrene
(discontinued **) Polystyrene 680 is a medium impact polystyrene developed for the foam extrusion and laminate markets. This polymers impact qualities in conjunction with its high flexural strength allow 680 to be ex.. |