Mechanical Properties Metric English Comments
Falling Dart Impact 0.678 J
0.500 ft-lb
ASTM D3029
Total 680 Polystyrene  (discontinued **)
Polystyrene 680 is a medium impact polystyrene developed for the foam extrusion and laminate markets. This polymers impact qualities in conjunction with its high flexural strength allow 680 to be ex..