Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | >= 1.99 J @Temperature 23.0 °C |
>= 1.47 ft-lb @Temperature 73.4 °F |
Internal |
AKG Polymers Vision PP PPH BL1302 T20 Polypropylene Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Falling Dart Impact | >= 1.99 J @Temperature 23.0 °C |
>= 1.47 ft-lb @Temperature 73.4 °F |
Internal |
AKG Polymers Vision PP PPH BL3004 Polypropylene Homopolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Falling Dart Impact | >= 1.99 J @Temperature 23.0 °C |
>= 1.47 ft-lb @Temperature 73.4 °F |
Internal |
AKG Polymers Vision PP PPH BL5003 Polypropylene Homopolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Falling Dart Impact | >= 1.99 J @Temperature 23.0 °C |
>= 1.47 ft-lb @Temperature 73.4 °F |
Internal |
AKG Polymers Vision PP PPH Jazz0502dark Polypropylene Homopolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Falling Dart Impact | >= 1.99 J @Temperature 23.0 °C |
>= 1.47 ft-lb @Temperature 73.4 °F |
Internal |
AKG Polymers Vision PP PPH TC3004 Polypropylene Homopolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |