Mechanical Properties Metric English Comments
Falling Dart Impact >= 1.99 J

@Temperature 23.0 °C
>= 1.47 ft-lb

@Temperature 73.4 °F
Internal
AKG Polymers Vision PP PPH BL1302 T20 Polypropylene Compound
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin..
Falling Dart Impact >= 1.99 J

@Temperature 23.0 °C
>= 1.47 ft-lb

@Temperature 73.4 °F
Internal
AKG Polymers Vision PP PPH BL3004 Polypropylene Homopolymer Compound
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin..
Falling Dart Impact >= 1.99 J

@Temperature 23.0 °C
>= 1.47 ft-lb

@Temperature 73.4 °F
Internal
AKG Polymers Vision PP PPH BL5003 Polypropylene Homopolymer Compound
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin..
Falling Dart Impact >= 1.99 J

@Temperature 23.0 °C
>= 1.47 ft-lb

@Temperature 73.4 °F
Internal
AKG Polymers Vision PP PPH Jazz0502dark Polypropylene Homopolymer Compound
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin..
Falling Dart Impact >= 1.99 J

@Temperature 23.0 °C
>= 1.47 ft-lb

@Temperature 73.4 °F
Internal
AKG Polymers Vision PP PPH TC3004 Polypropylene Homopolymer Compound
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin..