Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 176 J @Temperature -40.0 °C |
130 ft-lb @Temperature -40.0 °F |
F50; ASTM D3056 |
A. Schulman LP481 Molding Grade High-Density Polyethylene DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman. |
|||
Falling Dart Impact | 176 J @Temperature -40.0 °C |
130 ft-lb @Temperature -40.0 °F |
F50; ASTM D3056 |
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou.. |
|||
Falling Dart Impact | 176 J @Temperature -40.0 °C |
130 ft-lb @Temperature -40.0 °F |
F50; ASTM D3056 |
A. Schulman LP481 Molding Grade High-Density Polyethylene DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman. |
|||
Falling Dart Impact | 176 J @Temperature -40.0 °C |
130 ft-lb @Temperature -40.0 °F |
F50; ASTM D3056 |
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou.. |
|||
Falling Dart Impact | 176 J @Temperature -40.0 °C |
130 ft-lb @Temperature -40.0 °F |
F50; ASTM D3056 |
A. Schulman LP481 Molding Grade High-Density Polyethylene DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman. |
|||
Falling Dart Impact | 176 J @Temperature -40.0 °C |
130 ft-lb @Temperature -40.0 °F |
F50; ASTM D3056 |
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou.. |
|||
Falling Dart Impact | 176 J @Temperature -40.0 °C |
130 ft-lb @Temperature -40.0 °F |
F50; ASTM D3056 |
A. Schulman LP481 Molding Grade High-Density Polyethylene DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman. |
|||
Falling Dart Impact | 176 J @Temperature -40.0 °C |
130 ft-lb @Temperature -40.0 °F |
F50; ASTM D3056 |
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou.. |
|||
Falling Dart Impact | 176 J @Temperature -40.0 °C |
130 ft-lb @Temperature -40.0 °F |
F50; ASTM D3056 |
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou.. |
|||
Falling Dart Impact | 176 J @Temperature -40.0 °C |
130 ft-lb @Temperature -40.0 °F |
F50; ASTM D3056 |
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou.. |
|||
Falling Dart Impact | 176 J @Temperature -40.0 °C |
130 ft-lb @Temperature -40.0 °F |
F50; ASTM D3056 |
A. Schulman LP481 Molding Grade High-Density Polyethylene DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman. |
|||
Falling Dart Impact | 176 J @Temperature -40.0 °C |
130 ft-lb @Temperature -40.0 °F |
F50; ASTM D3056 |
A. Schulman LP481 Molding Grade High-Density Polyethylene DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman. |