Mechanical Properties Metric English Comments
Falling Dart Impact 29.8 J
22.0 ft-lb
73°F; ASTM D3029
Spartech GELOY SP-6730 Weatherable Sheet
Description: Weatherable SheetGeloy is a registered trademark of General Electric Company.Information provided by Spartech.
Falling Dart Impact 29.8 J
22.0 ft-lb
73°F; ASTM D3029
Spartech Weather-Pro Weatherable Sheet
Description: Weatherable SheetInformation provided by Spartech.