Polymer Property : Falling Dart Impact = 27.8 J
Polymer Property :
Falling Dart Impact =
27.8 J
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Falling Dart Impact
27.8
J
20.5
ft-lb
73°F; ASTM D3029
Spartech Millennium IV Glass Filled ABS Structural Sheet
Description: Structural SheetInformation provided by Spartech.