Spartech Millennium IV Glass Filled ABS Structural Sheet

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Sheet
Manufacturer Spartech
Trade Name Millennium
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Millennium IV Glass Filled ABS Structural Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Structural SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength, Yield 37.5 MPa
5440 psi
ASTM D638
Flexural Yield Strength 62.7 MPa
9100 psi
ASTM D790
Flexural Modulus 1.99 GPa
289 ksi
ASTM D790
Falling Dart Impact 27.8 J
20.5 ft-lb
73°F; ASTM D3029
Thermal Properties Metric English Comments
CTE, linear 59.4 µm/m-°C

@Temperature 20.0 °C
33.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 93.9 °C
201 °F
ASTM D648
Optical Properties Metric English Comments
Gloss 90 %
90 %
Gardner; ASTM D2523