Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 0.570 - 4.10 J | 0.420 - 3.02 ft-lb | Average value: 2.55 J Grade Count:5 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |