Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 75.9 - 75.9 J @Temperature -40.0 - -40.0 °C |
56.0 - 56.0 ft-lb @Temperature -40.0 - -40.0 °F |
Average value: 75.9 J Grade Count:1 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |