Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 0.903 - 20.0 MPa | 131 - 2900 psi | Average value: 8.71 MPa Grade Count:24 |
Overview of materials for PVC, Foam Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Foam Grade". Each property range of values reported is minimum and maximum values of appropriate Ma.. |