Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | >= 1.70 MPa | >= 247 psi | ASTM D3574E |
Rogers Corporation Poron® 4701-60-30 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4.. |
|||
Tensile Strength, Ultimate | 1.70 - 33.0 MPa | 247 - 4790 psi | Average value: 17.8 MPa Grade Count:59 |
Overview of materials for Styrene/Butadiene/Styrene (SBS) This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Butadiene/Styrene (SBS)". Each property range of values reported is minimum and maximum values o.. |
|||
Tensile Strength, Ultimate | 1.70 MPa | 247 psi | |
Kuraray HYBRAR® F1 Foam Compound Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Tensile Strength, Ultimate | 1.70 - 281 MPa | 247 - 40800 psi | Average value: 122 MPa Grade Count:706 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |