Polymer Property : Tensile Strength, Ultimate = 33.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3.40 - 33.0 MPa
493 - 4790 psi
Average value: 15.2 MPa Grade Count:52
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a..
Tensile Strength, Ultimate 9.20 - 33.0 MPa
1330 - 4790 psi
Average value: 18.9 MPa Grade Count:13
Overview of materials for Medium Density Polyethylene (MDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim..
Tensile Strength, Ultimate 1.70 - 33.0 MPa
247 - 4790 psi
Average value: 17.8 MPa Grade Count:59
Overview of materials for Styrene/Butadiene/Styrene (SBS)
This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Butadiene/Styrene (SBS)". Each property range of values reported is minimum and maximum values o..
Tensile Strength, Ultimate 27.0 - 33.0 MPa
3920 - 4790 psi
Average value: 29.0 MPa Grade Count:3
Overview of materials for Nylon 612, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Impact Modified". Each property range of values reported is minimum and maximum values of app..