Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 1.79 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1.79 MPa
260 psi
Across Flow; ASTM D412
ExxonMobil Vyram™ 9101-55 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
Tensile Strength, Ultimate 1.79 MPa
260 psi
cured 90 days @ 25°C
Abatron AboCast/AboCure 8110-3 Flexible Epoxy
This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic..
Tensile Strength, Ultimate 1.79 MPa
260 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 8211-55M300 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and ..
Tensile Strength, Ultimate 1.79 MPa
260 psi
Across Flow; ASTM D412
ExxonMobil Vyram™ 9201-55 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
Copyright © lookpolymers.com All Rights Reserved