Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1008 MPa | 146200 psi | |
Kennametal Stellite Stellite® 6K 12.7 or 22.2 mm plate 13.3 mm^3 volume loss--abrasive wear data. Applications include agitators, augers, ball mills, banbury mills, cams, crusher bearings, dryers, dry presses, dump cars, fans, filters, food machinery, g.. |