Tensile Strength, Ultimate 570 - 710 MPa
82700 - 103000 psi
SSAB Tunnplat Docol® 500YP High-strength Steel
High-strength SteelComments: Docol YP - Cold Rolled Steel - HSLA. Property values are for cold-rolled steel; thicknesses 0.5 - 3.00 mm. Iron content is approximate - exact composition is not report..
Tensile Strength, Ultimate 607 - 710 MPa
88000 - 103000 psi
Eagle Brass 510 Phosphor Bronzes 5% A, Extra Hard
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
Tensile Strength, Ultimate 648 - 710 MPa
94000 - 103000 psi
Ametek High Purity Nickel Strip 899A Full Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Tensile Strength, Ultimate 648 - 710 MPa
94000 - 103000 psi
Ametek High Purity Nickel Strip 899L Full Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Tensile Strength, Ultimate 648 - 710 MPa
94000 - 103000 psi
Ametek High Purity Nickel Strip 899M Full Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..