Polymer Property : Tensile Strength, Ultimate = 10900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 65.0 - 75.0 MPa
9430 - 10900 psi
Average value: 68.7 MPa Grade Count:16
Overview of materials for Polycarbonate, Gamma Radiation Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum..
Tensile Strength, Ultimate 29.0 - 75.0 MPa
4210 - 10900 psi
Average value: 58.4 MPa Grade Count:31
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Tensile Strength, Ultimate 60.0 - 75.0 MPa

@Temperature 130 - 175 °C
8700 - 10900 psi

@Temperature 266 - 347 °F
Average value: 69.4 MPa Grade Count:2
Overview of materials for Nylon 6, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea..
Tensile Strength, Ultimate 60.0 - 75.0 MPa

@Time 1.80e+7 - 7.20e+7 sec
8700 - 10900 psi

@Time 5000 - 20000 hour
Average value: 69.4 MPa Grade Count:2
Overview of materials for Nylon 6, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea..