Polymer Property : Tensile Strength, Ultimate = 11100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 76.5 MPa
11100 psi
Cotronics 4700 Ultra Temp Adhesive and Casting Epoxy, General Purpose
Tensile Strength, Ultimate 76.5 MPa
11100 psi
5mm/min; ASTM D638
Asia International Enterprise (Hong Kong) 6010FGN Nylon 66
Information provided by Asia International Enterprise (Hong Kong) Ltd.
Tensile Strength, Ultimate 76.5 MPa
11100 psi
5mm/min; ASTM D638
Asia International Enterprise (Hong Kong) 60T6F Nylon 66, 30% Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.