Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 76.5 MPa | 11100 psi | |
Cotronics 4700 Ultra Temp Adhesive and Casting Epoxy, General Purpose |
|||
Tensile Strength, Ultimate | 76.5 MPa | 11100 psi | 5mm/min; ASTM D638 |
Asia International Enterprise (Hong Kong) 6010FGN Nylon 66 Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Tensile Strength, Ultimate | 76.5 MPa | 11100 psi | 5mm/min; ASTM D638 |
Asia International Enterprise (Hong Kong) 60T6F Nylon 66, 30% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |