Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 121 MPa
17500 psi
ASTM D638
Nylene® Vexel™ B12GF30 SA , 30% Glass Reinforced PBT
Description: Vexel™ B12GF30 SA is a 30% glass fiber reinforced PBT with improved surface aPolyphenylene Etherarance. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are..
Tensile Strength, Ultimate 121 MPa
17500 psi
ISO value at 5mm/min.
BASF Capron® GR40 HS 40% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)
Capron GR40 HS is a heat stabilized 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stabil..
Tensile Strength, Ultimate 121 MPa
17500 psi
ASTM Data
Dow Questra® QA802 High Heat Syndiotactic Polystyrene, 30% Glass Filled  (discontinued **)
QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve..
Tensile Strength, Ultimate 121 MPa
17500 psi
ASTM Data
Dow Questra® WA205 High Heat Syndiotactic Polystyrene, 30% Glass Filled  (discontinued **)
QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve..
Tensile Strength, Ultimate 121 MPa
17500 psi
ASTM Data
Dow Questra® WA550 High Heat Syndiotactic Polystyrene, 30% Glass Filled  (discontinued **)
QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve..
Tensile Strength, Ultimate 121 - 207 MPa
17500 - 30000 psi
Average value: 158 MPa Grade Count:7
Overview of materials for Nylon 11 + Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp..
Tensile Strength, Ultimate 121 MPa
17500 psi
5 mm/min
Arkema Group Rilsan® AZM 30 O TLD Nylon 12, 30% Glass Fiber Filled (Dry)
Designation ISO 1874-PA12,MHLR,16-050,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: natural. Light and heat stabilizing agent. Mold-release agent.High rigidity. High..
Tensile Strength, Ultimate 121 MPa
17500 psi
AIM 80In/Pb15/Ag5 Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.
Tensile Strength, Ultimate 121 MPa
17500 psi
ASTM D638
Chem Polymer Durlex 730 G PBT, 30% Glass Fiber Reinforced
A lubricated 30% glass reinforced PBT offering a balance of dimensional stability, tensile strength and high temperature performance.Data provided by the manufacturer, Chem Polymer.
Tensile Strength, Ultimate 121 MPa
17500 psi
ASTM D638
A. Schulman ComAlloy Comtuf® 630 Nylon 6/6, Glass Reinforced, Impact Modified, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int..
Tensile Strength, Ultimate 121 MPa
17500 psi
ASTM D638
A. Schulman ComAlloy Hiloy® 413 Polyester - PBT, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Tensile Strength, Ultimate 121 MPa
17500 psi
ASTM D638
Chem Polymer Formax 630 G Acetal, 30% Glass Fiber Reinforced
A copolymer acetal reinforced with 30% glass fiber for use in applications requiring great strength and rigidity.Data provided by the manufacturer, Chem Polymer.
Tensile Strength, Ultimate 121 MPa
17500 psi
ISO value at 5mm/min.
BASF Capron® GR40 40% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)
Capron GR40 is a 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is also ava..
Tensile Strength, Ultimate 121 MPa
17500 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Lubri-Tech™ NI-10CF/15T Nylon 6/10, Carbon Fiber Reinforced, PTFE Lubricated  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Ultimate 121 MPa
17500 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® NI-20GF/000 Nylon 6/10, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Ultimate 121 MPa
17500 psi
ASTM D638
PolyOne Lubri-Tech™ ES-20GF/08T Polyethersulfone - 20% Glass Fiber And PTFE  (discontinued **)
Data provided by PolyOne.
Tensile Strength, Ultimate 121 MPa
17500 psi
ASTM D638
PolyOne Lubri-Tech™ ES-20GF/15T Polyethersulfone - 20% Glass Fiber Reinforced - 15% PTFE Lubricated  (disconti
Data provided by PolyOne.