Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.10 - 1.28 g/cc
0.0397 - 0.0462 lb/in³
Average value: 1.19 g/cc Grade Count:7
Filler Content 25.0 - 40.0 %
25.0 - 40.0 %
Average value: 30.0 % Grade Count:3
Water Absorption 0.150 %
0.150 %
Average value: 0.150 % Grade Count:3
Additive Loading 15.0 - 25.0 %
15.0 - 25.0 %
Average value: 21.3 % Grade Count:4
Linear Mold Shrinkage 0.000500 - 0.00300 cm/cm
0.000500 - 0.00300 in/in
Average value: 0.00150 cm/cm Grade Count:7
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 121 - 207 MPa
17500 - 30000 psi
Average value: 158 MPa Grade Count:7
Elongation at Break 1.00 - 5.50 %
1.00 - 5.50 %
Average value: 3.18 % Grade Count:7
Modulus of Elasticity 7.24 - 22.8 GPa
1050 - 3300 ksi
Average value: 13.4 GPa Grade Count:7
Flexural Yield Strength 186 - 276 MPa
27000 - 40000 psi
Average value: 225 MPa Grade Count:7
Flexural Modulus 6.55 - 17.2 GPa
950 - 2500 ksi
Average value: 11.1 GPa Grade Count:7
Izod Impact, Notched 0.961 - 2.14 J/cm
1.80 - 4.00 ft-lb/in
Average value: 1.40 J/cm Grade Count:7
Izod Impact, Unnotched 5.34 - 10.7 J/cm
10.0 - 20.0 ft-lb/in
Average value: 8.12 J/cm Grade Count:7
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 193 - 235 °C
380 - 455 °F
Average value: 216 °C Grade Count:3
Deflection Temperature at 1.8 MPa (264 psi) 188 - 232 °C
370 - 450 °F
Average value: 210 °C Grade Count:4
Flammability, UL94 HB
HB
Grade Count:7
Electrical Properties Metric English Comments
Electrical Resistivity 0.100 - 10.0 ohm-cm
0.100 - 10.0 ohm-cm
Average value: 5.39 ohm-cm Grade Count:4
Processing Properties Metric English Comments
Processing Temperature 216 - 282 °C
420 - 540 °F
Average value: 249 °C Grade Count:3
Melt Temperature 224 - 288 °C
435 - 550 °F
Average value: 256 °C Grade Count:4
Mold Temperature 37.8 - 65.6 °C
100 - 150 °F
Average value: 51.7 °C Grade Count:7
Drying Temperature 79.4 °C
175 °F
Average value: 79.4 °C Grade Count:4
Moisture Content 0.200 %
0.200 %
Average value: 0.200 % Grade Count:4
Dew Point -17.8 °C
0.000 °F
Average value: -17.8 °C Grade Count:4
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:7
Copyright © lookpolymers.com All Rights Reserved