Tensile Strength, Ultimate 122 MPa
17700 psi
ASTM Data
Dow Questra® EA514 High Heat Syndiotactic Polystyrene, 40% Glass Filled  (discontinued **)
QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve..
Tensile Strength, Ultimate 122 MPa
17700 psi
dry; ISO 527-1/-2
DSM Novamid® 1010GN2-15 NAT PA6-GF15 FR(17)
15% Glass Reinforced, Flame Retardant, Injection Molding, High Flow
Tensile Strength, Ultimate 122 MPa
17700 psi
5mm/min; ISO 527
BASF Ultramid® A3EG3 BK00564 15% Glass Filled PA66 (Dry)
Ultramid A3EG3 BK00564 is a 15% glass fiber reinforced injection molding PA66 grade. It conforms to FDA requirements of 21 CFR 177.1500.
Tensile Strength, Ultimate 122 MPa
17700 psi
5mm/min; ISO 527
BASF Ultramid® B3GM35 BKQ649 23220 15/25% Glass/Mineral Filled PA6 (Dry)
Ultramid B3GM35 BKQ649 23220 is a 40% combined glass-fiber and mineral reinforced, pigmented black injection molding PA6 grade.