Polymer Property : Tensile Strength, Ultimate = 1235 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 8.515 MPa
1235 psi
post cured- 4 hours at 177°C; ASTM D412
Multibase C6-530 Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Ultimate 8.515 MPa
1235 psi
ASTM D638
Ecomass® 4703ZC87 Stainless Steel Filled Polyurethane
Nontoxic alternative to Lead (Pb), weighting and balancing applicationsModerate Specific GravityStainless Steel Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polymers