Polymer Property : Tensile Strength, Ultimate = 12600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 87.0 MPa

@Temperature 60.0 °C
12600 psi

@Temperature 140 °F
ISO 527
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
Tensile Strength, Ultimate 87.0 MPa
12600 psi
5 mm/min
Arkema Group Orgalloy® RS 6015 BV Nylon 6 Alloy, Glass Fiber + Bead Filled (Conditioned)
RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties..
Tensile Strength, Ultimate 87.0 MPa
12600 psi
ASTM D638
A. Schulman ComAlloy Hiloy® 436 Glass/Mineral Reinforced, PBT Alloy
Data provided by the manufacturer, ComAlloy International Company.20% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.