Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman ComAlloy Hiloy® 436 Glass/Mineral Reinforced, PBT Alloy

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass + Mineral Filled
Manufacturer A. Schulman ComAlloy
Trade Name Hiloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Hiloy® 436 Glass/Mineral Reinforced, PBT Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.20% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 114
114
ASTM D785
Tensile Strength, Ultimate 87.0 MPa
12600 psi
ASTM D638
Elongation at Break 3.7 %
3.7 %
ASTM D638
Flexural Strength 138 MPa
20000 psi
ASTM D790
Flexural Modulus 5.70 GPa
827 ksi
ASTM D790
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.23 J/cm
9.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 210 - 225 °C
410 - 437 °F
Deflection Temperature at 0.46 MPa (66 psi) 221 °C
430 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
Copyright © lookpolymers.com All Rights Reserved