Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 8.929 MPa | 1295 psi | ASTM D412; ISO 37 |
Advanced Polymer Alloys DuraGrip™ DGR 6140 UT Thermoplastic Elastomer (TPE) DuraGrip® DGR 6140UT is an unfilled translucent Thermoplastic Elastomer (TPE). It is designed to process easily in injection molding and extrusion applications. DuraGrip® TPE
features excellent so.. |