Polymer Property : Tensile Strength, Ultimate = 134 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 45.0 - 134 MPa
6530 - 19500 psi
Average value: 76.3 MPa Grade Count:23
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu..