Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 20.7 - 96.0 MPa
3000 - 13900 psi
Average value: 65.0 MPa Grade Count:14
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum ..
Tensile Strength, Ultimate 78.0 - 96.0 MPa
11300 - 13900 psi
Dow CYCLOTENE™ 4022-35 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ 4022-35 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Tensile Strength, Ultimate 78.0 - 96.0 MPa
11300 - 13900 psi
Dow CYCLOTENE™ 4024-40 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ 4024-40 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Tensile Strength, Ultimate 78.0 - 96.0 MPa
11300 - 13900 psi
Dow CYCLOTENE™ 4026-46 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ 4026-46 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Tensile Strength, Ultimate 78.0 - 96.0 MPa
11300 - 13900 psi
Dow CYCLOTENE™ XU35075 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ XU35075 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Tensile Strength, Ultimate 78.0 - 96.0 MPa
11300 - 13900 psi
Dow CYCLOTENE™ XU35132 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ XU35132 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Tensile Strength, Ultimate 78.0 - 96.0 MPa
11300 - 13900 psi
Dow CYCLOTENE™ XU35133 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ XU35133 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Tensile Strength, Ultimate 90.0 - 96.0 MPa
13100 - 13900 psi
Typical
ATI Allegheny Ludlum AL 20™ Sheet and Strip Specialty Steel
The N08020 alloy has been available for many years and has found applications in many environments, such as in chlorides and in sulfuric and sulfurous acids.Although AL 20 alloy was developed for im..