Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 8460 Shield Adapter Kit

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 8460 Shield Adapter Kit.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M Shield Adapter Kits are designed to accommodate the grounding of accessories installed on conventional Tape, Longitudinally Corrugated (LC), Wire and UniShield power cables. The shield Adapter Kit design provides a fault current capacity of 600 amps on 15 through 35 kV class cables.Information provided by 3M
Physical Properties Metric English Comments
Moisture Absorption 1.80 %
1.80 %
7 days at 90°C in water
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 9.65 MPa
1400 psi
ASTM D412-75
Elongation at Break 750 %
750 %
ASTM D412-75
300% Modulus 0.00331 GPa
0.480 ksi
ASTM D412-75
Tear Strength 26.3 kN/m
150 pli
Die C; ASTM D624-73
Electrical Properties Metric English Comments
Dielectric Strength 11.1 kV/mm
282 kV/in
7 days in water at 90°C; ASTM D149-75
14.4 kV/mm

@Thickness 1.78 mm
365 kV/in

@Thickness 0.0700 in
Original; ASTM D149-75
Descriptive Properties Value Comments
Appearance Black
Users viewing this material also viewed the following: