Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1007 MPa
146100 psi
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 1.6 mm thick sheet
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Tensile Strength, Ultimate 1007 MPa

@Temperature 649 °C
146100 psi

@Temperature 1200 °F
Kennametal Stellite Stellite® 6K 1.6 mm thick sheet
13.3 mm^3 volume loss--abrasive wear data. Applications include agitators, augers, ball mills, banbury mills, cams, crusher bearings, dryers, dry presses, dump cars, fans, filters, food machinery, g..
Tensile Strength, Ultimate 1007 MPa
146100 psi
Haynes Ultimet® alloy, aged 1000 hours at 649°C (1200°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Tensile Strength, Ultimate 1007 MPa
146100 psi
Haynes Hastelloy® C-22® alloy, GMAW, as welded, notched
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..