Material Notes:
13.3 mm^3 volume loss--abrasive wear data. Applications include agitators, augers, ball mills, banbury mills, cams, crusher bearings, dryers, dry presses, dump cars, fans, filters, food machinery, galvanizing roll necks, grinder ring bearings, marine equipment, mixing equipment, pulleys, pump seals, pump shafts, rotary kilns, scraper rolls, screw conveyors, spindles, stuffing boxes, thickeners, tile presses, wear bars. Data provided by the manufacturer, Deloro Stellite Inc.Product of former Deloro Stellite Inc.
Physical Properties Metric English Comments
Density 8.387 g/cc
0.3030 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1217 MPa
176500 psi
120 MPa

@Temperature 1090 °C
17400 psi

@Temperature 2000 °F
235 MPa

@Temperature 982 °C
34100 psi

@Temperature 1800 °F
484 MPa

@Temperature 816 °C
70200 psi

@Temperature 1500 °F
1007 MPa

@Temperature 649 °C
146100 psi

@Temperature 1200 °F
Tensile Strength, Yield 708 MPa

@Strain 0.200 %
103000 psi

@Strain 0.200 %
59.0 MPa

@Strain 0.200 %,
Temperature 1090 °C
8560 psi

@Strain 0.200 %,
Temperature 2000 °F
133 MPa

@Strain 0.200 %,
Temperature 982 °C
19300 psi

@Strain 0.200 %,
Temperature 1800 °F
307 MPa

@Strain 0.200 %,
Temperature 816 °C
44500 psi

@Strain 0.200 %,
Temperature 1500 °F
Elongation at Break 4.0 %
4.0 %
in 50.8 mm
8.0 %

@Temperature 649 °C
8.0 %

@Temperature 1200 °F
in 50.8 mm
17 %

@Temperature 816 °C
17 %

@Temperature 1500 °F
in 50.8 mm
28 %

@Temperature 982 °C
28 %

@Temperature 1800 °F
in 50.8 mm
53 %

@Temperature 1090 °C
53 %

@Temperature 2000 °F
in 50.8 mm
Thermal Properties Metric English Comments
CTE, linear 13.8 µm/m-°C

@Temperature 0.000 - 400 °C
7.67 µin/in-°F

@Temperature 32.0 - 752 °F
13.8 µm/m-°C

@Temperature 0.000 - 200 °C
7.67 µin/in-°F

@Temperature 32.0 - 392 °F
13.8 µm/m-°C

@Temperature 0.000 - 100 °C
7.67 µin/in-°F

@Temperature 32.0 - 212 °F
13.8 µm/m-°C

@Temperature 0.000 - 500 °C
7.67 µin/in-°F

@Temperature 32.0 - 932 °F
14.0 µm/m-°C

@Temperature 0.000 - 600 °C
7.78 µin/in-°F

@Temperature 32.0 - 1110 °F
14.2 µm/m-°C

@Temperature 0.000 - 700 °C
7.89 µin/in-°F

@Temperature 32.0 - 1290 °F
14.5 µm/m-°C

@Temperature 0.000 - 800 °C
8.06 µin/in-°F

@Temperature 32.0 - 1470 °F
14.9 µm/m-°C

@Temperature 0.000 - 900 °C
8.28 µin/in-°F

@Temperature 32.0 - 1650 °F
15.5 µm/m-°C

@Temperature 0.000 - 1000 °C
8.61 µin/in-°F

@Temperature 32.0 - 1830 °F
Melting Point 1265 - 1354 °C
2309 - 2469 °F
Solidus 1265 °C
2309 °F
Liquidus 1354 °C
2469 °F
Component Elements Properties Metric English Comments
Carbon, C 1.4 - 1.9 %
1.4 - 1.9 %
Chromium, Cr 28 - 32 %
28 - 32 %
Cobalt, Co 49.1 - 55.6 %
49.1 - 55.6 %
As remainder
Iron, Fe <= 3.0 %
<= 3.0 %
Manganese, Mn <= 2.0 %
<= 2.0 %
Molybdenum, Mo <= 1.5 %
<= 1.5 %
Nickel, Ni <= 3.0 %
<= 3.0 %
Silicon, Si <= 2.0 %
<= 2.0 %
Tungsten, W 3.5 - 5.5 %
3.5 - 5.5 %
Electrical Properties Metric English Comments
Magnetic Permeability <= 1.20

@Temperature 22.0 °C
<= 1.20

@Temperature 71.6 °F
200 Oersted (15.900 A/m)