Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 15.4 MPa | 2230 psi | |
Freudenberg Simrit E425 Hydrocarbon Elastomer Excellent resistance to water, steam and polar solvents, as well as ozone and sunlight. Also resistant to alcohols, glycol engine coolants and SKY-DROL (phosphate ester hydraulic fluid). Avoid n.. |
|||
Tensile Strength, Ultimate | 15.4 MPa | 2230 psi | Air aged 14 days at 175°C |
DuPont Vamac® GLS Sample Compound Vulcanizate Slab Cured Test slab is press cured for 5 minutes at 177°C and post cured for 4hrs at 175°C. Vulcanizate performance test data can help end-users evaluate the potential fitness of similar compounds for thei.. |
|||
Tensile Strength, Ultimate | 15.4 MPa | 2230 psi | Cured 10 minutes at 180°C |
DuPont Vamac® DP 5.5 phr Peroxide Test Compound Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper.. |
|||
Tensile Strength, Ultimate | 15.4 MPa | 2240 psi | |
Colorite Polymers Flexchem 6551-02 Vinyl Compound Description: The Flexchem "51" series is a group of translucent, flexible, non-toxic vinyl compounds which were specifically developed to replace silicone in various applications. These compounds ut.. |