Polymer Property : Tensile Strength, Ultimate = 1500 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1500 MPa
218000 psi
International Mold Steel Premium H13 Hot Work Die and Mold Steel
Description: International Mold Steel's Premium H-13 is a chromium-based, hot work die and plastic mold steel designed for increased production rates and longer tool life. It meets the restricti..
Tensile Strength, Ultimate 1500 MPa
218000 psi
Haynes 242® alloy, cold reduced sheet, annealed and 40% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Tensile Strength, Ultimate 1500 MPa

@Temperature -196 °C
218000 psi

@Temperature -320 °F
Universal Wire Works 6Al-4V (ELI) (AMS 4956) Titanium Alloy Filler Metal
Universal titanium alloy 6Al-4V (ELI) is similar to type 6Al-4V in chemical analysis with the exception of Extra Low Interstitial gases (ELI). By controlling these contaminating gases the fracture t..
Tensile Strength, Ultimate 1500 MPa
218000 psi
Perpendicular to Thickness
Zircar Ceramics Alumina Mat
A layered, low density flexible mat made of 100% polycrystalline alumina fiber (non-RCF) designed for use to temperatures as high as 1650°C (3002°F). Shot free low density mat used as fill between..
Tensile Strength, Ultimate 1500 MPa
218000 psi
at HRC 45
Bohler-Uddeholm UDDEHOLM MIRRAX ESR Plastic Mold Steel
Uddeholm Mirrax ESR is specially developed and adapted for larger molds that require corrosion resistance and/or high surface finish.It is characterized by:High hardenability for consistent properti..
Tensile Strength, Ultimate 1500 MPa
218000 psi
after hot stamping
ArcelorMittal Usibor® 1500 Ultra high strength steel, Cold Rolled
Description: Usibor® 1500 and 22MnB5 are hot formed grades intended for use in automobile structural and safety components. The very high mechanical strength of the final part makes it possible to ..
Tensile Strength, Ultimate 1500 MPa
218000 psi
after hot stamping
ArcelorMittal Usibor® 1500 Ultra high strength steel, Hot Rolled
Description: Usibor® 1500 and 22MnB5 are hot formed grades intended for use in automobile structural and safety components. The very high mechanical strength of the final part makes it possible to ..
Tensile Strength, Ultimate 1500 MPa
218000 psi
after hot stamping
ArcelorMittal Usibor® 22MnB5 Ultra high strength steel, Cold Rolled
Description: Usibor® 1500 and 22MnB5 are hot formed grades intended for use in automobile structural and safety components. The very high mechanical strength of the final part makes it possible to ..
Tensile Strength, Ultimate 1500 MPa
218000 psi
after hot stamping
ArcelorMittal Usibor® 22MnB5 Ultra high strength steel, Hot Rolled
Description: Usibor® 1500 and 22MnB5 are hot formed grades intended for use in automobile structural and safety components. The very high mechanical strength of the final part makes it possible to ..