Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Universal Wire Works 6Al-4V (ELI) (AMS 4956) Titanium Alloy Filler Metal

Category Metal , Nonferrous Metal , Titanium Alloy , Alpha/Beta Titanium Alloy
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 6Al-4V (ELI) (AMS 4956) Titanium Alloy Filler Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Universal titanium alloy 6Al-4V (ELI) is similar to type 6Al-4V in chemical analysis with the exception of Extra Low Interstitial gases (ELI). By controlling these contaminating gases the fracture toughness is greatly increased. Alloy 4956 is used to weld liquid hydrogen tankage and airframe parts requiring a high fracture toughness.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 896 MPa
130000 psi
1500 MPa

@Temperature -196 °C
218000 psi

@Temperature -320 °F
Tensile Strength, Yield 827 MPa

@Strain 0.200 %
120000 psi

@Strain 0.200 %
1390 MPa

@Strain 0.200 %,
Temperature -196 °C
202000 psi

@Strain 0.200 %,
Temperature -320 °F
Elongation at Break 10 %
10 %
13.5 %

@Temperature -196 °C
13.5 %

@Temperature -320 °F
Component Elements Properties Metric English Comments
Aluminum, Al <= 6.75 %
<= 6.75 %
Carbon, C <= 0.030 %
<= 0.030 %
Hydrogen, H <= 0.0050 %
<= 0.0050 %
Iron, Fe <= 0.20 %
<= 0.20 %
Manganese, Mn <= 0.10 %
<= 0.10 %
Nitrogen, N <= 0.012 %
<= 0.012 %
Other <= 0.10 %
<= 0.10 %
Oxygen, O <= 0.080 %
<= 0.080 %
Titanium, Ti >= 88.273 %
>= 88.273 %
As Remainder
Vanadium, V <= 4.5 %
<= 4.5 %