Polymer Property : Tensile Strength, Ultimate = 1552 MPa
Polymer Property :
Tensile Strength, Ultimate =
1552 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Ultimate
1552
MPa
225100
psi
Zoltek Panex 30® High Twist Carbon Roving
High Twist Carbon RovingApplications include: Friction Clutches & Brakes, Composite Substructures