Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1570 MPa
228000 psi
510°C Temper Temperature
Latrobe Lescalloy® D6AC VAC-ARC High Strength Alloy Steel
LESCALLOY D6AC VAC-ARC steel is a medium carbon, low alloy, ultra high strength steel primarily designed for high strength structural applications requiring strength leaves up to 280,000 psi. This ..
Tensile Strength, Ultimate 1570 MPa
228000 psi
SSAB Tunnplat Domex® 034 BOR Oil quenched Boron Steel
Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex® high strength steels offers a number of ..