Material Notes:
Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex® high strength steels offers a number of benefits compared to ordinary structural steels: Lower weight, Simpler production, Lower creep rate, Longer useful life, Higher load-bearing capacity, Lower transport costs, Reduced stocks, Lower overall cost.Data provided by SSAB Tunnplat.
Physical Properties Metric English Comments
Density 7.87 g/cc
0.284 lb/in³
Estimated by MatWeb
Mechanical Properties Metric English Comments
Hardness, Vickers 480
480
HV<sub>10</sub>; approximate
Tensile Strength, Ultimate 1570 MPa
228000 psi
Tensile Strength, Yield 1030 MPa
149000 psi
Elongation at Break 10 %
10 %
A<sub>5</sub>
Impact 20
20
J/cm²; -20°C
30
30
J/cm²; 20°C
Component Elements Properties Metric English Comments
Boron, B 0.0030 %
0.0030 %
Carbon, C 0.25 - 0.30 %
0.25 - 0.30 %
Chromium, Cr 0.15 - 0.25 %
0.15 - 0.25 %
Iron, Fe 98 %
98 %
As Remainder
Manganese, Mn 1.0 - 1.3 %
1.0 - 1.3 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Silicon, Si 0.20 - 0.35 %
0.20 - 0.35 %
Sulfur, S <= 0.025 %
<= 0.025 %
Users viewing this material also viewed the following: