Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 160 MPa
23200 psi
Osprey Metals CE17 Al-Si Controlled Expansion Alloy
Al-27%Si controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals.
Tensile Strength, Ultimate 160 MPa
23200 psi
ASTM D638
Owens Corning Glass Fiber Reinforced Nylon 6/6, 30 wt.% glass
Nylons, as a group, are inert to most organic solvents. They resist alkalis and salt solutions and they are attacked by strong mineral acids and oxidizing agents. Data provided by the manufacturer,..
Tensile Strength, Ultimate 160 MPa
23200 psi
Same value from ASTM and ISO tests; 5 mm/min.
BASF Capron® SEG6 H1 30% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron SEG6 H1 is a 30% glass reinforced nylon 6 injection molding compound. This material is currently under development as XA-2678. It exhibits exceptional surface aesthetics at the slower fill s..
Tensile Strength, Ultimate 160 MPa
23200 psi
ISO 527
LATI LARPEEK 50 G/30 30% Glass Reinforced Polyetheretherketone (PEEK)  (Unverified Data**)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
Tensile Strength, Ultimate 160 MPa
23200 psi
ASTM D638
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide Compound  (Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® R-4 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at..
Tensile Strength, Ultimate 160 MPa
23200 psi
ASTM D638
Firestone CG430-001 Nylon 6, 30% Fiberglass Filled
Natural color. Heat stabilized. Fiber size is 4 mm length and 14 µm diameter.Information provided by Firestone
Tensile Strength, Ultimate 160 MPa

@Temperature 22.0 °C
23200 psi

@Temperature 71.6 °F
25mm flat samples, compression moulded; ISO 527-4
Menzolit Menzolit® SMC 1800 Unsaturated Polyester UP
SMC 1800 is for structural applications requiring extreme high mechanical properties and low weight. These compounds mould to parts focussing on mechanical strength for replacement of metals in ord..
Tensile Strength, Ultimate 160 MPa

@Temperature 1095 °C
23200 psi

@Temperature 2003 °F
Haynes 25 alloy, cold rolled and 1205°C (2200°F) solution annealed sheet
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Ultimate 160 MPa
23200 psi
dry; ISO 527-1/-2
DSM Novamid® 1010GN2-30 NAT/BK37 PA6-GF30 FR(17)
30% Glass Reinforced, Flame Retardant
Tensile Strength, Ultimate 160 MPa
23200 psi
dry; ISO 527-1/-2
DSM Stanyl® TW242FM10 PA46-(GF+MF)50
50% Glass/Mineral Reinforced, Heat Stabilized
Tensile Strength, Ultimate 160 MPa
23200 psi
cond; ISO 527-1/-2
DSM Stanyl® TW272B6 (PA46+PTFE)-CF30
30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified
Tensile Strength, Ultimate 160 MPa
23200 psi
5 mm/min
Arkema Group Orgalloy® RS 6635 A Nylon 66 Alloy, 35% Glass Fiber (Conditioned)
RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie..
Tensile Strength, Ultimate 160 MPa
23200 psi
ISO R527
Arkema Group Orgalloy® RS 6635 A Polyamide 6.6 Alloy 35% Glass Fiber reinforced
Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group
Tensile Strength, Ultimate 160 MPa

@Temperature 871 °C
23200 psi

@Temperature 1600 °F
Carpenter Gall-Tough PLUS™ Stainless, Annealed
Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 4..
Tensile Strength, Ultimate 160 MPa
23200 psi
ASTM D638
Adell WR-37 33% Glass Reinforced PET
Tensile Strength, Ultimate 160 MPa
23200 psi
ASTM data at 5 mm/min.
BASF Capron® 8232G HS BK-102 25% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8232G HS BK-102 is a pigmented black, heat stabilized, 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional..
Tensile Strength, Ultimate 160 MPa
23200 psi
ASTM data at 5 mm/min.
BASF Capron® 8232G HS FR 25% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant nylon 6 injection molding compound exhibiting excellent melt stability characteristics. It combines flame retard..
Tensile Strength, Ultimate 160 MPa
23200 psi
ASTM D638
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide Compound  (Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® BR111 is a glass and mineral filled polyphenylene sulfide compounds developed to provide a good combination of mechanical strength and electrical ..
Tensile Strength, Ultimate 160 MPa
23200 psi
ISO 527
Solvay Specialty Polymers Primef® 4002 40% GF PPS, High Fluidity Grade  (discontinued **)
Used for injection molding of high performance parts.
Tensile Strength, Ultimate 160 MPa
23200 psi
cond; ISO 527-1/-2
DSM Stanyl® TS200F10 PA46-GF50
50% Glass Reinforced
Tensile Strength, Ultimate 160 MPa
23200 psi
ASTM D638
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 50 wt.% glass
Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u..