Polymer Property : Tensile Strength, Ultimate = 1890 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 9.00 - 13.0 MPa
1310 - 1890 psi
ASTM D412
Multibase Multi-Flex® TPE A 8502 BLK
The fogging test value is 90% according to ASTM SAE-J275. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tensile Strength, Ultimate 8.00 - 13.0 MPa
1160 - 1890 psi
Average value: 10.2 MPa Grade Count:7
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Compounding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Compounding Grade". Each property range of values reported is minimu..