Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1438 MPa | 208600 psi | Longitudinal |
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 900 AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, .. |