Polymer Property : Tensile Strength, Ultimate = 2090 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 14.4 MPa
2090 psi
ASTM D638
DuPont 20 Series 20-6064 Specialty Polyethylene Resin
DuPont 20-6064 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding..
Tensile Strength, Ultimate 14.4 MPa
2090 psi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4760P Compound
FormulationNordel® IP 4760P