Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 13.7 - 21.6 MPa
1990 - 3130 psi
ASTM D638
Polikim EFALON® B-60 PTFE, 60% Bronze Filled
Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing..