Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polikim EFALON® B-60 PTFE, 60% Bronze Filled

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Bronze Filled
Manufacturer Polikim Polimer ve Kimya Sanay
Trade Name EFALON®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polikim EFALON® B-60 PTFE, 60% Bronze Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearings, piston rings, valve sets, valve components.Information provided by Polikim Polimer.
Physical Properties Metric English Comments
Density 3.80 - 4.00 g/cc
0.137 - 0.145 lb/in³
ASTM D792
Deformation 1.0 - 1.1 %

@Temperature 150 °C,
Time 86400 sec,
Pressure 0.981 MPa
1.0 - 1.1 %

@Temperature 302 °F,
Time 24.0 hour,
Pressure 142 psi
total
1.5 - 2.0 %

@Temperature 23.0 °C,
Time 86400 sec,
Pressure 13.7 MPa
1.5 - 2.0 %

@Temperature 73.4 °F,
Time 24.0 hour,
Pressure 1990 psi
permanent; ASTM D621
3.7 - 4.8 %

@Temperature 23.0 °C,
Time 86400 sec,
Pressure 13.7 MPa
3.7 - 4.8 %

@Temperature 73.4 °F,
Time 24.0 hour,
Pressure 1990 psi
total; ASTM D621
9.0 - 10 %

@Temperature 150 °C,
Time 86400 sec,
Pressure 4.90 MPa
9.0 - 10 %

@Temperature 302 °F,
Time 24.0 hour,
Pressure 711 psi
total
Mechanical Properties Metric English Comments
Hardness, Shore D 65 - 70
65 - 70
ASTM D2240
Tensile Strength, Ultimate 13.7 - 21.6 MPa
1990 - 3130 psi
ASTM D638
Elongation at Break 110 - 220 %
110 - 220 %
ASTM D638
Compressive Strength 10.3 - 10.8 MPa
1490 - 1560 psi
1% Deformation; ASTM D695
Izod Impact, Notched (ISO) 10.0 - 11.0 kJ/m²
4.76 - 5.23 ft-lb/in²
ASTM D256
Coefficient of Friction 0.13
0.13
Coefficient of Friction, Static 0.070
0.070
Limiting Pressure Velocity 0.004905 - 0.005232 MPa-m/sec
140.0 - 149.4 psi-ft/min
3 m/min
0.00638 - 0.00654 MPa-m/sec
182 - 187 psi-ft/min
30 m/min
0.00736 - 0.00900 MPa-m/sec
210 - 257 psi-ft/min
300 m/min
Thermal Properties Metric English Comments
CTE, linear 75.0 - 90.0 µm/m-°C

@Temperature 25.0 - 100 °C
41.7 - 50.0 µin/in-°F

@Temperature 77.0 - 212 °F
ASTM D696
100 - 115 µm/m-°C

@Temperature 25.0 - 200 °C
55.6 - 63.9 µin/in-°F

@Temperature 77.0 - 392 °F
ASTM D696
130 - 140 µm/m-°C

@Temperature 25.0 - 300 °C
72.2 - 77.8 µin/in-°F

@Temperature 77.0 - 572 °F
ASTM D696
Thermal Conductivity 0.711 - 0.837 W/m-K
4.93 - 5.80 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 270 °C
518 °F
continuous
Minimum Service Temperature, Air -260 °C
-436 °F
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+7 ohm-cm
>= 1.00e+7 ohm-cm
ASTM D257
Surface Resistance >= 1.00e+9 ohm
>= 1.00e+9 ohm
50% rel. humidity; ASTM D257