Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 215 MPa
31200 psi
5mm/min; ISO 527
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Dry)
Ultramid 8234G HS is a heat stabilized, 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensio..